Equipment sourcing · Raw materials
Buying road bitumen for Africa: grade, testing and hot logistics
Bitumen is not something to buy by the tonne without further detail. Its grade governs how a pavement copes with heat and traffic, and its logistics are unusual: it travels and is handled hot, with burn risks and a violent reaction if it meets water. For a roads authority, a public works agency or a contractor bidding on a donor-funded contract, both aspects belong in the purchasing file.
Sobetracom neither refines nor stocks bitumen. From Belgium, we turn the design office's prescription into a purchase specification, approach refiners and distributors able to supply the required grade, compare their offers against the same tests and organise document checks and inspection before shipment.
Updated on 21 October 2026
Penetration grades under EN 12591
In Europe, penetration-grade paving bitumens fall under EN 12591. The name gives the penetration range at 25 °C in tenths of a millimetre: a 50/70 is a bitumen into which the standard needle sinks by 50 to 70 tenths. As Eurobitume explains, the EN 1426 test measures how far a 100 g needle penetrates in 5 seconds at 25 °C. The lower the figure, the harder the bitumen.
ExxonMobil's data sheet shows the usual market range: 20/30, 35/50, 50/70, 70/100 and 160/220. The grade is chosen in the pavement design, according to service temperatures, traffic and the asphalt mix, not from a catalogue. Our job is to make sure each offer covers that exact grade rather than a neighbouring one that happens to be easier to source.
What the specification should state
Penetration alone is not enough. The ring and ball softening point (EN 1427) describes behaviour at high service temperatures, which matters a great deal in a hot climate. For a 35/50, LOTOS gives a softening point of 50-58 °C, a Fraass breaking point no higher than -5 °C, a flash point of at least 240 °C and solubility of at least 99%. ExxonMobil quotes 46-54 °C for its 50/70 and 43-51 °C for its 70/100.
The specification should also call for tests after RTFOT ageing (EN 12607-1), which simulates mixing and the transport of hot asphalt. For the LOTOS 35/50: mass change of 0.5% at most, retained penetration of at least 53% and a softening point increase of no more than 8 °C. For every lot we ask for the refinery's test certificate and declaration of performance, and check them against the specification limits before dispatch.
Modified binders need their own tests
For roads carrying heavy goods traffic, the design office may prescribe polymer-modified bitumen. Eurobitume notes that modification aims to improve properties such as flexibility or stiffness and is usually achieved by adding synthetic polymers. These binders are checked with specific tests, such as elastic recovery (EN 13398) or force ductility (EN 13589).
A modified binder is more sensitive to long hot storage and to mix homogeneity, so offers should also be compared on the time between production and use, and on the storage conditions planned all the way to site.
Hot logistics and the risks that come with it
Bitumen is handled hot. Eurobitume states that handling generally takes place above 100 °C, and its storage guidance still recommends 125 °C for a 35/50 and 120 °C for a 50/70 when a tank has to be kept full for a short period. Burns from splashes or spills are the main hazard. Nynas points to another risk that the rainy season makes worse: water reaching hot bitumen vaporises instantly and causes a violent boil-over. A badly closed tank or a damp drum is enough to trigger it.
The delivery mode is decided with the site team: hot bulk where heated tanks and suitable access exist, or packaged bitumen reheated on site for remote works. Either way, the supplier's safety instructions, the safety data sheets and operators' protective equipment are part of the purchase.
Frequently asked questions
- Can a 70/100 replace a specified 50/70?
- No. A 70/100 is softer: ExxonMobil gives it a softening point of 43-51 °C, against 46-54 °C for its 50/70. Under high temperatures and heavy traffic, that difference affects rutting. Only the design office can approve a substitution.
- Which documents should accompany each bitumen lot?
- The lot test certificate showing penetration, softening point and post-RTFOT results, the refinery's declaration of performance and the safety data sheet. Any national requirements in the destination country, and the tests the client's laboratory will repeat on receipt, should be agreed with the project owner before ordering.
Sources
- Grupa LOTOS (ORLEN), fiche « Road bitumen 35/50 » (October 2026)
- ExxonMobil, fiche produit « Paving Bitumen EM » (France) (October 2026)
- Eurobitume, « Bitumen: technical » (October 2026)
- Eurobitume, « Bitumen: HSE » (October 2026)
- Eurobitume, « Guidance for the Storage of Bitumen », septembre 2023 (September 2023)
- Nynas, « Bitumen: Safety » (October 2026)
This page summarises public sources as of the date shown. It does not replace the official text: check it before committing to a purchase, a bid or a shipment.