Equipment sourcing · Raw materials
Buying steel for a project in Africa: grades, mill certificates and shipping
A tender that simply asks for "steel" invites bids that cannot be compared. A beam, a plate and a reinforcing bar fall under different standards and different tests, and lots sold under the same grade name can arrive with very different quality paperwork. For a ministry, an NGO or a contractor building in Africa, the value of a steel purchase lies as much in the specification as in the price.
Sobetracom is neither a mill nor a stockholder. From Belgium, we turn the project's needs into a specification, approach qualified producers and distributors, compare their offers on the same basis and have the lot inspected before it leaves. The pointers below come from European standards and producers' data sheets; the standard set by the project owner always takes precedence.
Updated on 20 October 2026
Sections and plate: state the full EN 10025-2 grade
For structural sections and plate, the European reference is EN 10025-2, covering non-alloy structural steels. The figure after the S is the minimum yield strength in MPa for thinner material: Arvedi's data sheet gives at least 235 MPa for S235JR, 275 MPa for S275JR and 355 MPa for S355J2 up to 16 mm, with lower values above that.
The suffix sets the impact test temperature: the same 27 J minimum applies at 20 °C for JR, 0 °C for J0 and -20 °C for J2. Writing "S355" without the quality lets the supplier pick the cheapest option. The same sheet maps EN grades to legacy names, which helps when an old drawing still says St 37-2 or ASTM A283; the specification should name the EN grade and say whether any equivalent is acceptable.
Rebar: ductility matters as much as strength
B500A, B500B and B500C all share a characteristic yield strength of 500 MPa. What separates them is the Rm/Re ratio and the total elongation at maximum force (Agt). According to The Concrete Centre, B500B requires a ratio of 1.08 and 5.0% elongation, while B500C requires a ratio between 1.15 and 1.35 and 7.5% elongation. A less ductile B500A is no substitute where the design assumes B500B.
The underlying European standard, EN 10080, is listed as withdrawn, so each country relies on its own texts: BS 4449 in the UK, national approvals elsewhere. Mills reflect this, and Feralpi lists separate country certifications for its B500B bars. Before going to tender, find out which reference the destination's building control body accepts and ask the producer for matching evidence.
A type 3.1 certificate tied to the actual lot
Since its 2004 revision, EN 10204 recognises only types 2.1, 2.2, 3.1 and 3.2. Types 2.1 and 2.2 are issued by the manufacturer itself. A 3.1 certificate reports specific test results on the lot and is validated by a manufacturer's representative who is independent of production. A 3.2 adds the signature of the buyer's representative or an inspector designated by regulation.
For structural steel we ask for a 3.1 at the very least, showing the heat number, chemical analysis and mechanical tests, and we check that the heat number matches the marking on the bars or sections. Where a donor requires it, an inspection body appointed by the buyer witnesses the tests and signs a 3.2. That decision belongs before the tender, since it affects the schedule.
Salt water, heat and humidity on the way to site
Steel ships as breakbulk or in containers depending on tonnage and lengths, and water is the main threat. Marine insurer The Swedish Club notes that seawater oxidises steel about 10 times faster than fresh water. It recommends a pre-loading survey with dated photographs and silver nitrate tests, followed by hold ventilation based on dew points. That survey is what any later claim for a corroded lot will rest on.
On site, Bangladesh's building code, written for a monsoon climate, offers rules that travel well: bars and sections on supports, at least 200 mm off the ground for long storage or coastal sites, types and diameters kept apart, and bar ends painted a colour per type. Written into the delivery plan, they stop crews cutting full-length bars because the right ones cannot be found.
Frequently asked questions
- Is a type 2.2 test report enough for rebar on a public building?
- A 2.2 is a report of non-specific tests issued by the manufacturer; it does not prove that the delivered lot was tested. For public or donor-funded works, a 3.1 tied to the heat number is a sensible minimum, and the project owner may require a 3.2.
- Can we accept a grade described as "equivalent" to the one on the drawings?
- Only if the equivalence is written down and can be checked. Producers' cross-reference tables match designations, but equivalence is about chemistry and test results, not the name. We have the design office approve it before an offer is retained, and the destination country's standard still needs confirming with its building control body.
Sources
- Arvedi, « Non-alloyed structural steels as per EN 10025-2 », fiche produit (October 2026)
- The Concrete Centre, « Standards for reinforcement » (October 2026)
- Feralpi Stahl, « Reinforcing bars hot rolled and hot rolled cold formed » (October 2026)
- Wermac, « EN 10204 Certificate Types » (October 2026)
- The Swedish Club, « Cargo Advice: Steel cargoes » (December 2023)
- Bangladesh National Building Code 2012, Part 7, Chapter 2 « Storage, Stacking and Handling Practices » (2012)
This page summarises public sources as of the date shown. It does not replace the official text: check it before committing to a purchase, a bid or a shipment.